Parameters:

Category

Item

Index

Component

VAC/VeoVa/E

 

 

Properties

Appearance

White powder

Solid content, %

99 ± 1

Stacking density, g/l

450 - 600

Ash content (burning under 1000 ℃), %

10 ± 2

PH value

6 - 8

Lowest film forming temperature, ℃

0

Glass transition temperature,℃

0 ± 3

Security

Non - toxic

Packaging

Multi - layer of paper bag

25 kg/bag

Usages:
This product belongs to polymer powders polymerized by vinyl acetate, advanced fatty acid vinyl ester and ethylene and has good flexibility. It can be dispersed in water, enhance the adhesion strength between mortar and supports and improve the mechanical properties of mortar. The film of model HW-5116 has good flexibility, strength and plasticity, wear resistance and strong deformation ability. Moreover, HW-5116 is able to effectively enhance the bending and tensile resistance of materials in polymer cement mortar and therefore its crack resistance is good enough to prevent materials from cracking effectively.

Applications:
Insulation (EPS, XPS) mortar
Plastering (anti - crack) mortar
Waterproof mortar
Insulation system
Flexible putty of external wall
Flexible thin - layer mortar
Wearable floor
Concrete repair
Wall plaster
Bonding mortar
Interface agent
Caulked joint paste
Interior or exterior paint

 

Packaging and storage:
It is packed in paper bags enclosed plastic bag. The net weight is 25kg/bag.
It must be stored in a cool, dry place and the unused part shall be sealed as soon as possible after opening the bag in case of moisture absorption.
Its useful life is 6 months and it should be used as early as possible under high temperature and wet conditions to avoid increasing the agglomeration probability.
Because of the thermoplasticity of the powder, the stacked height of the product is not allowed exceeding one tray.

Total0bar [View All]  Related Comments
 
More>other products

[ ProductsSearch ]  [ Send Fav ]  [ Share ]  [ Print ]  [ Send Report ]  [ Close ]

 
Home | Products | Suppliers | News | Tradeshow | Sitemap | Message | RSS Feed